DATE | HS_CODE | Product Description | Trademark | Country | Net Weight | Statistical Cost | Place | Shipper Name | Consignee Name |
---|
2017-08-15 | 2713120009 | Samples calcined petroleum coke (calcined). Ash content: 0.3-0.5%, sulfur: 0,6-3,6%. Designed for laboratory research. | *** | SWITZERLAND | 25 | 1 | *** | ***** | ***** |
2017-08-18 | 2713120009 | KOKS OIL calcined. WEIGHT, based on 0.1% of the moisture-427000KG. : MOISTURE CONTENT-no more than 0.1% of sulfur, not exceeding 2.0%. It is used in the electrolysis. | *** | CHINA | 427000 | 105689,14 | DOSTYK | ***** | ***** |
2017-08-21 | 2713120009 | Petroleum coke PROKALENNY. WEIGHT, based on 0.1% of the moisture-534105KG. : MOISTURE CONTENT-no more than 0.1% of sulfur, not exceeding 2.0%. It is used in the electrolysis. | *** | CHINA | 544900 | 131818,6 | DOSTYK | ***** | ***** |
2017-09-05 | 2713120009 | OIL SAMPLES calcined KOKSA.PREDNAZNACHENY for laboratory tests. : Soda, Contents: ASH-0,22-0.25%, sulfur-05, -1,83%, a true density 2,09-2,11G / cm3. | *** | INDIA | 10 | *** | *** | ***** | ***** |
2017-09-06 | 2713120009 | OIL SAMPLES calcined KOKSA.PREDNAZNACHENY for laboratory tests. : Soda, Contents: ASH-0,22-0.25%, sulfur-05, -1,83%, a true density 2,09-2,11G / cm3. | *** | INDIA | 10.05 | *** | *** | ***** | ***** |
2017-09-08 | 2713120009 | Calcined petroleum coke of the anode in chamber furnaces, ash marks ECP-2. GET OUT OF CRUDE OIL anodic / electrode coke IGNITION in chamber furnaces. TU 0258-003-00149452-96 C MOD. 5: Use the aluminum industry for | *** | RUSSIA | 1000000 | 78405,39 | Seaport of Ust Luga | ***** | ***** |
2017-09-18 | 2713120009 | Calcined petroleum coke of the anode in chamber furnaces, ash marks ECP-2. GET OUT OF CRUDE OIL anodic / electrode coke IGNITION in chamber furnaces. TU 0258-003-00149452-96 C MOD. 5: Use the aluminum industry for | *** | RUSSIA | 9000000 | 700834,47 | Seaport of Ust Luga | ***** | ***** |
2017-09-21 | 2713120009 | Calcined petroleum coke of the anode in chamber furnaces, ash marks ECP-2. GET OUT OF CRUDE OIL anodic / electrode coke IGNITION in chamber furnaces. TU 0258-003-00149452-96 C MOD. 5 USED IN ALUMINUM INDUSTRY FOR OUT | *** | *** | 500000 | 38536,44 | Seaport of Ust Luga | ***** | ***** |
2017-09-25 | 2713120009 | Calcined petroleum coke. WEIGHT, based on 0.1% of the moisture-303696KG. : MOISTURE CONTENT-no more than 0.1% of sulfur, not exceeding 2.0%. It is used in the electrolysis. | *** | CHINA | 304000 | 82573,73 | DOSTYK | ***** | ***** |
2017-09-26 | 2713120009 | Samples calcined petroleum coke (calcined). Ash content: 0.3-0.5%, sulfur: 0.6-3.0%. Designed for laboratory research. | *** | SWITZERLAND | 5.5 | 0,17 | *** | ***** | ***** |