DATE | HS_CODE | Product Description | Trademark | Country | Net Weight | Statistical Cost | Place | Shipper Name | Consignee Name |
---|
2017-09-04 | 3802900000 | Diatomaceous filter GRADE POWDER RS1000, in an amount of 40 TONN.MINERALNAYA sedimentary rocks RECEIVED open method, followed by purification and KLASSIFIKATSIEY.POSLE WHAT IS MADE calcination-FIRING WITH FLUX (sintered DOBAVKA-: CARBON | *** | CHINA | 40000 | 16400 | *** | ***** | ***** |
2017-09-05 | 2818200000 | ALUMINUM OXIDE, OTHER THAN ARTIFICIAL CORUNDUM: calcined alumina obtained by calcination (sintering) in a drum oven at TEMPETURE 1400-1600 GRAD.TSELSIYA calcined alumina, CHEMICAL ANALYSIS: AL2O3 ~ 99%, NA2O - 0.08-0.012% | *** | *** | 44000 | 91221,09 | *** | ***** | ***** |
2017-09-05 | 2818101100 | ALUMINA. PRODUCTION PROCESS: MILL OF METALLURGICAL ALUMINA, washing, cleaning, calcination, drying, milling. DESIGNED to produce high quality refractories. Dispersing alumina. FACTION: 2.5, 2.6, 7.5, 7.9. MIC. CHEM. Comp | *** | GERMANY | 17150 | 32590,77 | *** | ***** | ***** |
2017-09-06 | 8414594000 | "SUPPLY tertiary air into the furnace for coke calcination" is delivered in parts, for their own use are not intended for alienation. Is a set of equipment installed on the housing calcining AVAILABLE: PE | *** | INDIA | 13739 | 772542,14 | *** | ***** | ***** |
2017-09-07 | 2818200000 | ALUMINUM OXIDE, OTHER THAN ARTIFICIAL CORUNDUM: calcined alumina obtained by calcination (sintering) in a drum oven at TEMPETURE 1400-1600 GRAD.TSELSIYA JET GLINOZEM.HIMICHESKY ANALYSIS: AL2O3 ~ 99%, NA2O - 0.07-0.08%, FE2O3 - | *** | GERMANY | 20000 | 44148,38 | *** | ***** | ***** |
2017-09-07 | 2818101100 | Artificial corundum used in the manufacture of refractories are dense sintered alumina crystals SOSTYASCHY OF ALPHA-Al2O3 (corundum) ALUMINA obtained by calcination at a temperature exceeding 1500 GRAD. : Basic compounds are O | *** | CHINA | 18000 | 24928,11 | *** | ***** | ***** |
2017-09-08 | 3802900000 | Diatomaceous filter GRADE POWDER RS700, in an amount of 40 TONN.MINERALNAYA sedimentary rocks RECEIVED open method, followed by purification and KLASSIFIKATSIEY.POSLE WHAT IS MADE calcination-FIRING WITH FLUX (sintered DOBAVKA-: CARBONIFEROUS | *** | CHINA | 40000 | 16400 | *** | ***** | ***** |
2017-09-09 | 3802900000 | Mineral products Activated: Activated kieselguhr (diatomaceous earth, which was held wet cleaning, drying, calcination, activation during firing in the rotary kiln FOR EXPANDING particles to the desired size), packed in bags. Diatomaceous earth, the coarse fraction | *** | *** | 20700 | 16228,92 | *** | ***** | ***** |
2017-09-11 | 2818200000 | Aluminum oxide (calcined alumina) other than synthetic corundum, prepared by calcination at ALUMINA HIGH TEMPERATURE WET obtained by processing bauxite METHOD Bayer, CASâ„–1344-28-1. Calcined alumina APPLY KA | *** | SPAIN | 68100 | 38614,05 | *** | ***** | ***** |
2017-09-12 | 2710129008 | Preservatives COMPOUND dewatering, MARK SOCOPAC 65H, cartridges X 500 ml for rustproofing PARTS DURING STORAGE; MARK .: 020-68936011: Ingredients: DISTILLATES OIL LIGHT - 75% petrolatum OIL - 5%, the calcination of salt - 5% B | *** | FRANCE | 7 | 546,61 | *** | ***** | ***** |