DATE | HS_CODE | Product Description | Trademark | Country | Net Weight | Statistical Cost | Place | Shipper Name | Consignee Name |
---|
2017-11-09 | 3214101009 | Polysulfide SEALANT P / N PR1773 A2, PCS 10, for sealing seams, COMPOSITION. Polysulfide polymer 50% -100%, 2.5-10% CALCIUM CARBONATE, TITANIUM DIOXIDE 2.5-10%, 2.5-10 TOLUENE % orthophosphate 0-2.5%, 0-2.5% butanone, zinc oxide 0-2.5%, 0-2.5% thiram, use | LJF | GERMANY | 1.5 | 335,12 | EKATERINBURG | ***** | ***** |
2017-11-22 | 3214900009 | Polysulfide sealants for sealing joints P / N PS890 A2, PCS 9, COMPOSITION PART A: 30-60% manganese dioxide, hydrogenated terphenyl 30-60% TALC <5%, terphenyl <5 SAWL <5%, terphenyl <5% 1,3-diphenyl <5% tetrasulfide <5%, pre-packaged in plastic | LE JOINT FRANCE | FRANCE | 1.341 | 217,59 | EKATERINBURG | ***** | ***** |
2017-11-22 | 3214900009 | Polysulfide sealants for sealing joints P / N PS890 A2, PCS 21, COMPOSITION PART A: 30-60% manganese dioxide, hydrogenated terphenyl 30-60% TALC <5%, terphenyl <5 SAWL <5%, terphenyl <5% 1,3-diphenyl <5% tetrasulfide <5%, pre-packaged in plastic | LE JOINT FRANCE | FRANCE | 3.129 | 507,71 | EKATERINBURG | ***** | ***** |
2017-11-23 | 3214101009 | Polysulfide TWO COMPONENT SEALANT FOR SEALING JOINTS, P / N PR 1750 A2, two PCS. COMPOSITION PART A: Manganese dioxide 30 - 60%, terphenyl 10 -30% -10% 5 ZEOLITES, polyphenylene 3 - 7% TALC 1 - 5% carbon 1-5% magnesium carbonate 1 - 5%, terphenyl 1 - 5%, 1, | PPG | UNITED STATES | 0.3 | 44,72 | EKATERINBURG | ***** | ***** |
2017-11-23 | 3214101009 | Polysulfide SEALANT P / N PS 890 A2, PCS 10, COMPOSITION PART A: 20-50% manganese dioxide, 5-10% ZEOLITES, polyphenylenes, partially hydrogenated 5-10% TALC 1-4,9% CARBON 1-5 %, 1-5% terphenyl, 1,3-diphenylguanidine 0,1-2,2% BIS (piperidin thiocarbonyl) tetrasulfide | PPG | UNITED STATES | 1.5 | 242,18 | EKATERINBURG | ***** | ***** |