DATE | HS_CODE | Product Description | Trademark | Country | Net Weight | Statistical Cost | Place | Shipper Name | Consignee Name |
---|
2017-10-20 | 7216501000 | Corner equal- hot rolled, without further treatment, of unalloyed steel 3 CONTAINING C = 0.15-0.20%, MN = 0.46-0.65%, SI = 0.07-0.21%), with ultimate (tensile strength) -450-495 MPA) | ABSENT | GUINEA | 7480 | 5217,08 | SAINT PETERSBURG | ***** | ***** |
2017-10-20 | 7216509900 | Corner equal- hot rolled, without further treatment, of unalloyed steel 3 SP-5, CONTAINING C = 0.19%, MN = 0.61%, SI = 0.20%), with ultimate (tensile strength) -495 MPa) | ABSENT | GUINEA | 2710 | 1903,07 | SAINT PETERSBURG | ***** | ***** |
2017-10-20 | 7216311000 | CHANNELS hot rolled, without further treatment, of unalloyed steel 3 SP-5, CONTAINING C = 0.16-0.20%, MN = 0.48-0.63%, SI = 0.11-0.23%), with ultimate (tensile strength) -429-485 MPA) | ABSENT | GUINEA | 8985 | 6304,45 | SAINT PETERSBURG | ***** | ***** |
2017-10-20 | 7216319000 | CHANNELS hot rolled, without further treatment, of unalloyed steel 3 SP-5, CONTAINING C = 0.157-0.160%, MN = 0.56-0.57%, SI = 0.25-0.27%), with ultimate (tensile strength) -421-434 MPA) | ABSENT | GUINEA | 3815 | 3220,32 | SAINT PETERSBURG | ***** | ***** |
2017-10-20 | 7214995000 | Hot-rolled, without further treatment, of unalloyed steel 20 (containing C = 0.18-0.20%, MN = 0.41-0.48%, SI = 0.20-0.24%), with ultimate (tensile strength) -440-460 MPA) | ABSENT | GUINEA | 4798 | 4407,77 | SAINT PETERSBURG | ***** | ***** |
2017-10-20 | 7214993900 | Hot-rolled, without further treatment, of unalloyed steel 3 (containing C = 0.18-0.20%, MN = 0.51-0.61%, SI = 0.07-0.22%), with ultimate (tensile strength) -430-505 MPA) | ABSENT | GUINEA | 3803 | 2809,50 | SAINT PETERSBURG | ***** | ***** |
2017-10-20 | 7214997900 | Hot-rolled, without further treatment, of unalloyed steel 45 (containing C = 0.44-0.46%, MN = 0.56%, SI = 0.22-0.26%), with ultimate (tensile strength) -607-649 MPA) | ABSENT | GUINEA | 365 | 282,47 | SAINT PETERSBURG | ***** | ***** |
2017-10-20 | 7214997100 | Hot-rolled, without further treatment, of unalloyed steel 45 (containing C = 0.45-0.46%, MN = 0.56-0.6%, SI = 0.26-0.27%), with ultimate (tensile strength) -660 MPa) | ABSENT | GUINEA | 1320 | 1021,54 | SAINT PETERSBURG | ***** | ***** |