DATE | HS_CODE | Product Description | Trademark | Country | Net Weight | Statistical Cost | Place | Shipper Name | Consignee Name |
---|
2017-09-28 | 4703210009 | WOOD PULP SULPHATE BLEACHED softwood (composition: 80-100% PINE, 0-20% FIR FOR CELLULOSE MARKS SUPREME BY STORA ENSO, minimum brightness 84% ​​ISO, CONTAMINATION LEVEL MAX 35 MM2 / kg) obtained by digestion CHIPS IN | ABSENT | *** | 21998 | 12316,27 | UIMAHARJU MILLS | ***** | ***** |
2017-11-02 | 4703210009 | WOOD PULP SULPHATE BLEACHED softwood (composition: 80-100% PINE, 0-20% FIR FOR CELLULOSE MARKS SUPREME BY STORA ENSO, minimum brightness 84% ​​ISO, CONTAMINATION LEVEL MAX 35 MM2 / kg) obtained by digestion CHIPS IN | ABSENT | *** | 21974 | 12225,79 | UIMAHARJU MILLS | ***** | ***** |
2017-11-07 | 4703210009 | WOOD PULP SULPHATE BLEACHED softwood (composition: 80-100% PINE, 0-20% FIR FOR CELLULOSE MARKS SUPREME BY STORA ENSO, minimum brightness 84% ​​ISO, CONTAMINATION LEVEL MAX 35 MM2 / kg) obtained by digestion CHIPS IN | ABSENT | *** | 21969 | 12185,84 | UIMAHARJU MILLS | ***** | ***** |
2017-11-21 | 4703210009 | WOOD PULP SULPHATE BLEACHED softwood (composition: 80-100% PINE, 0-20% FIR FOR CELLULOSE MARKS SUPREME BY STORA ENSO, minimum brightness 84% ​​ISO, CONTAMINATION LEVEL MAX 35 MM2 / kg) obtained by digestion CHIPS IN | ABSENT | *** | 21957 | 12296,77 | UIMAHARJU MILLS | ***** | ***** |
2017-11-22 | 4703210009 | WOOD PULP SULPHATE BLEACHED softwood (composition: 80-100% PINE, 0-20% FIR FOR CELLULOSE MARKS SUPREME BY STORA ENSO, minimum brightness 84% ​​ISO, CONTAMINATION LEVEL MAX 35 MM2 / kg) obtained by digestion CHIPS IN | ABSENT | *** | 21960 | 12355,43 | UIMAHARJU MILLS | ***** | ***** |
2017-11-23 | 4703210009 | WOOD PULP SULPHATE BLEACHED softwood (composition: 10-30% PINE, 70-90% FIR FOR CELLULOSE MARKS SUPREME STRONG BY STORA ENSO, minimum brightness 84% ​​ISO, CONTAMINATION LEVEL MAX 35 MM2 / kg) obtained by digestion CHIPS | ABSENT | *** | 22048 | 12423,58 | UIMAHARJU MILLS | ***** | ***** |
2017-11-28 | 4703210009 | WOOD PULP SULPHATE BLEACHED softwood (composition: 80-100% PINE, 0-20% FIR FOR CELLULOSE MARKS SUPREME BY STORA ENSO, minimum brightness 84% ​​ISO, CONTAMINATION LEVEL MAX 35 MM2 / kg) obtained by digestion CHIPS IN | ABSENT | *** | 20044 | 11427,87 | UIMAHARJU MILLS | ***** | ***** |
2017-11-28 | 4703210009 | WOOD PULP SULPHATE BLEACHED softwood (composition: 80-100% PINE, 0-20% FIR FOR CELLULOSE MARKS SUPREME BY STORA ENSO, minimum brightness 84% ​​ISO, CONTAMINATION LEVEL MAX 35 MM2 / kg) obtained by digestion CHIPS IN | ABSENT | *** | 21953 | 12558,93 | UIMAHARJU MILLS | ***** | ***** |
2017-11-28 | 4703210009 | WOOD PULP SULPHATE BLEACHED softwood (composition: 80-100% PINE, 0-20% FIR FOR CELLULOSE MARKS SUPREME BY STORA ENSO, minimum brightness 84% ​​ISO, CONTAMINATION LEVEL MAX 35 MM2 / kg) obtained by digestion CHIPS IN | ABSENT | *** | 22003 | 12550,92 | UIMAHARJU MILLS | ***** | ***** |