DATE | HS_CODE | Product Description | Trademark | Country | Net Weight | Statistical Cost | Place | Shipper Name | Consignee Name |
---|
2017-09-04 | 3921903000 | Paper coated (impregnated) uncured phenol formaldehyde (synthetic) resins, without pictures, (composite material consisting of several components). Dry MATERIAL has the effect of fragility and broken at inflection at SWL BOOM | *** | GERMANY | 19959 | 51849,16 | *** | ***** | ***** |
2017-09-04 | 3921903000 | Paper impregnated (coating) of the uncured phenol formaldehyde (synthetic) resins, without pictures, (composite material consisting of several components). Dry MATERIAL has the effect of fragility and broken at inflection at SWL: BU | *** | GERMANY | 19897 | 60008,01 | *** | ***** | ***** |
2017-09-04 | 3921909000 | A film of polymer material (not for retail): "CM-PREG R- 55/1050 CP001 55W" polymeric reinforced non-porous material obtained through impregnating a chemically modified resins (phenolic resins / POLIVININILBUTIRAL) Spices | *** | GERMANY | 2833.9 | 58706,6 | *** | ***** | ***** |
2017-09-04 | 3921909000 | A film of polymer material (not for retail): "CM-PREG R- 55/1050 CP001 55W" polymeric reinforced non-porous material obtained through impregnating a chemically modified resins (phenolic resins / POLIVININILBUTIRAL) Spices | *** | GERMANY | 2833.9 | 58706,6 | *** | ***** | ***** |
2017-09-05 | 3921903000 | COMPOSITE MATERIAL consisting of paper coated (impregnated) phenol-formaldehyde resins, INTENDED FOR LINING plywood FROM unbleached pulp, the fast roll on 60 1450 rm; TOP LAYER DENSITY 115-125 g / m2 COLOR | *** | GERMANY | 19550 | 55198,1 | *** | ***** | ***** |
2017-09-05 | 3921903000 | Film impregnated with phenolic-formaldehyde resin on a paper basis, impregnation completely hides STRUCTURE OF PAPER PROPERTIES film is determined by properties of the resin, non-porous, Designed for the lamination of plywood TPS 427 SEMI FAST CON 1270: TPS 427 SEM | *** | GERMANY | 19428 | 55655,46 | *** | ***** | ***** |
2017-09-05 | 3921909000 | Honeycomb panel of rectangular shape, the size 2500 x 1250 mm, made of aramid paper coated with the heat-resistant phenol-formaldehyde resin. Resistant to high pressure, chemicals, shock, vibration. Designed to create Cell | *** | GERMANY | 5 | 4083,21 | *** | ***** | ***** |
2017-09-05 | 3921909000 | Honeycomb panel of rectangular shape, the size 2500 x 1250 mm, made of aramid paper coated with the heat-resistant phenol-formaldehyde resin. Resistant to high pressure, chemicals, shock, vibration. Designed to create Cell | *** | GERMANY | 5 | 4083,21 | *** | ***** | ***** |
2017-09-07 | 3921190000 | POWER TM OASIS OF porous polymer material - 5110 pcs, for bouquets, in a cardboard box 10-01028 POWER TM. OASIS from phenol-aldehyde resins 23,0H11,0H8,0 SIZE SM for bouquets, in a carton, ART .: (146 CDF.) "S | *** | GERMANY | 259.8 | 792,64 | MOSCOW | ***** | ***** |
2017-09-07 | 3921190000 | POWER TM OASIS OF porous polymer material - 5110 pcs, for bouquets, in a cardboard box 10-01028 POWER TM. OASIS from phenol-aldehyde resins 23,0H11,0H8,0 SIZE SM for bouquets, in a carton, ART .: (146 CDF.) "S | *** | GERMANY | 259.8 | 792,64 | MOSCOW | ***** | ***** |